Pipe in sizes according to ANSI/ASME

Seamless, stainless pipe in sizes according to ANSI/ASME. Our ANSI/ASME stainless steel pipe is delivered in random lengths or cut to fixed lengths.

Vill du veta mer?

Ring oss Mejla oss

Materials

The Sandvik program of ANSI/ASME seamless pipe includes austenitic stainless steels, duplex and super-duplex stainless steels and a high-alloy austenitic stainless steel.

List of materials

Sandvik grade UNS ASTM EN no.
Sandvik 3R12 S30403 / S30400 304L / 304 1.4306 / 1.4301
Sandvik 3R65 S31603 / S31600 316L / 316 1.4404 / 1.4401
SAF 2205™ S31803 / S32205 - 1.4462
SAF 2507® S32750 - 1.4410
Sandvik 2RK65 N08904 - 1.4539
Sandvik 254 SMO S31254 - 1.4547

Available online

This product can be ordered online via our self-service platform E-Track, where you can also see stocks, get prices and view your order history.

E-Track is currently available in selected European countries but we are working on expanding the availability.


ORDER IN E-TRACK


Stock program

Pipe is stocked according to ANSI/ASME B36.19.
OD = outside diameter, WT = wall thickness.

Stock standard items: C = Central warehouse (Europe), U = United States

OD
mm
WT
mm
in. Sch Kg/m Sandvik
3R12
Sandvik
3R65
Sandvik
SAF 2205
Sandvik
SAF 2507
Sandvik
2RK65
Sandvik
254 SMO
13.72 1.65 1/4 10S 0.50
C
C
- - - -
13.72 2.24 1/4 40S 0.64
C
C
- - - -
13.72 3.02 1/4 80S 0.81
C
C
- - - -
17.15 1.65 3/8 10S 0.64
C
C
- - - -
17.15 2.31 3/8 40S 0.86
C
C
- - - -
17.15 3.20 3/8 80S 1.12
C
C
- - - -
21.34 2.11 1/2 10S 1.02
C
C
-
C
C1)
-
21.34 2.77 1/2 40S 1.29
C, U
C, U
C
C
C1)
C
21.34 3.73 1/2 80S 1.65
C, U
C, U
C
- - -
26.67 2.11 3/4 10S 1.30
C
C
C
-
C1)
-
26.67 2.87 3/4 40S 1.71
C, U
C, U
C
C
-
C
26.67 3.91 3/4 80S 2.23
C, U
C, U
C
- -
33.40 2.77 1 10S 2.13
C, U
C, U
C
C
C1)
C
33.40 3.38 1 40S 2.54
C, U
C, U
C
C
C1)
C
33.40 4.55 1 80S 3.29
C, U
C, U
C
C
- -
33.40 6.352) 1 160 4.30
C, U
C, U
- - - -
42.16 2.77 10S 2.73
C
C
C
C
C1)
-
42.16 3.56 40S 3.44
C, U
C, U
C
-
C1)
-
42.16 4.85 80S 4.53
C, U
C
- - - -
42.16 6.352) 160 5.69
C, U
C
- - - -
48.26 2.77 10S 3.16
C, U
C, U
C
C
C C
48.26 3.68 40S 4.11
C, U
C, U
C
C, U
C
C
48.26 5.08 80S 5.49
C, U
C, U
C
C
- -
60.33 2.77 2 10S 3.99
C, U
C, U
C
C
-
C
60.33 3.91 2 40S 5.52
C, U
C, U
C
C, U
C
C
60.33 5.54 2 80S 7.60
C, U
C, U
C
C
- C
60.33 8.742) 2 160 11.29
C, U
C, U
C
- - -
73.03 3.05 10S 5.35
C, U
C
C
-
C
-
73.03 5.16 40S 8.77
C, U
C, U
C
-
C
-
73.03 7.01 80S 11.59
C, U
C, U
C
- - -
88.90 3.05 3 10S 6.56
C, U
C, U
C
C
C
C
88.90 5.49 3 40S 11.47
C, U
C, U
C
C, U
C
C
88.90 7.62 3 80S 15.51
C, U
C, U
C
- - C
88.90 11.132) 3 160 21.67
C
C, U
C
- - -
101.60 3.05 10S 7.53
C
C
- - - -
101.60 5.74 40S 13.78
C, U
C
- - - -
101.60 8.08 80S 18.92
C, U
C, U
- - - -
114.30 3.05 4 10S 8.50
C, U
C, U
C
C
- C
114.30 6.02 4 40S 16.32
C, U
C, U
C
C
C
C
114.30 8.56 4 80S 22.67
C, U
C, U
C
-
- C
114.30 13.492) 4 160 34.05
C, U
C
C
- - -
141.30 6.55 5 40S 22.10
C, U
C
- - - -
141.30 9.53 5 80S 31.44
C, U
C
- - - -
141.30 15.882) 5 160 49.87
C
C
- - - -
168.28 3.4 6 10S 14.04
C, U
C, U
- - - -
168.28 7.11 6 40S 28.69
C, U
C, U
C
C
- -
168.28 10.97 6 80S 43.21
C, U
C, U
- - - C
168.28 14.27 6 120 54.75 - -
C
- - -
168.28 18.262) 6 160 68.59
C
C
C
- - -
219.08 8.18 8 40S 43.20
C, U
C
C
C
- -
219.08 12.7 8 80S 65.63
C
C
- - - -
219.08 18.23 8 120 91.30 - -
C
- - -
219.08 23.012) 8 160 112.97
C
C
C
- - -

1) Tested acc. to ASTM A312 and AD2000-W2 Einbaurohre TÜV Bl. 421 incl. hot tensile test at +400ºC (752ºF).

2) ASME B36.10

Tolerances

For ASTM A312 and ASTM A790, acc. to ASTM A999

Size, mm Tolerance OD, mm
13.72-48.3 +0.4/-0.8
>48.3-114.3 +/- 0.8
>114.3-219.1 +1.6/-0.8

Tolerances on wall thickness

Size, mm Wall thickness, % WT/OD ratio
13.72-73.03 +20/-12.5 All
88.90-219.10 +22.5/-12.5 Less or equal to 0.05
88.90-219.10 +15/-12.5 Above 0.05

Product standards

Sandvik 3R12 (ASTM 304L), Sandvik 3R65 and 3R60 (ASTM 316L)

  • ASTM A312 incl. corrosion test acc. to ASTM A262 Pr.E.
  • NACE MR-0.175/ISO 15156
  • Tolerances and leak test acc. to ASTM A312/A999
  • NORSOK MDS-S01 (ASTM 316L)

SAF 2205™ (UNS S31803/S32205) and SAF 2507® (UNS S32750)

  • ASTM A790 incl. corrosion test acc. to ASTM G-48 Method A (SAF 2205 at 25ºC/77ºF, SAF 2507 at 50ºC/122ºF - both for 24 hours).
  • NORSOK MDS D-41 (SAF 2205)
  • NORSOK MDS D-51 (SAF 2507)

Sandvik 2RK65™ (UNS N08904)

ASTM A312. Sizes marked 2) are also tested acc. to AD2000-W2 Einbaurohre TÜV Bl. 421 incl. hot tensile test at +400ºC (752ºF).

Sandvik 254 SMO (UNS S31254)

  • ANSI B36.19
  • ASTM A-312, ASME SA-312
  • PED 2014/68/EU, EN 10216-5 TC1
  • NORSOK M-630 ED-6, NORSOK MDS R11 REV.5
  • IOGP S-563 DEC.2018, MDS IR111/ IR111S REV.01
  • NACE MR0175/ ISO 15156-3, NACE MR0103/ISO 17945-1