Downhole casing and production tubing in CRA (corrosion resistant alloys) such as duplex stainless steels and austenitic Fe- and Ni-base alloys, Groups 2, 3 and 4, API 5 CRA (ISO 13680). These materials are ideal to cope with the aggressive environments found in wells sour from hydrogen sulfide, carbon dioxide and other chemicals.

Vill du veta mer?

Ring oss Mejla oss

Predominantly, Sandvik's downhole casing and tube material is supplied in the cold-worked condition to ensure high strength and weight effective design solutions.

Sandvik carries five grade alternatives for plain end pipe for downhole casing, production tubing and coupling stock. Please contact us for a reference list of Sandvik's products for OCTG and downhole applications.

List of materials (other grades can be offered on request)
Sandvik grade Grade description
SAF 2205™
(22Cr, UNS S31803/ S32205)
SAF 2205™ / 22Cr is a duplex stainless steel, which is resistant to CO2 -corrosion and to sour corrosion at low partial pressures of H2S.
SAF 2507®
(25Cr, UNS S32750)
SAF 2507® / 25Cr is a super-duplex stainless steel similar to SAF 2205™ / 22Cr, but with slightly improved H2S resistance and significantly higher resistance to chloride-induced corrosion.
SAF 3207 HD™ (UNS S33207) SAF 3207 HD™ is a hyper-duplex stainless steel with exceptional strength and excellent resistance to stress corrosion cracking (SCC) in hydrogen sulfide (H2S) and chloride containing environments.
Sanicro® 28
(UNS N08028)
Sanicro® 28 is a high alloy stainless steel comparable with Alloy 825. It has excellent resistance to corrosion in severe downhole environments, especially to high partial pressures of H2S and high chloride contents.
Sanicro® 29 For very high chloride contents in combination with high partial pressures of H2S. Sanicro® 29 provides even better resistance to localized corrosion and sulfide stress cracking compared to Sanicro® 28.
Sanicro® 48 As an austenitic nickel-base alloy for highly corrosive OCTG downhole applications, Sanicro® 48 is characterized by its excellent resistance to sulfide stress cracking, stress corrosion cracking (SCC) in chloride, and sour (H2S/Cl) environments and its very high resistance to pitting and crevice corrosion.
Mechanical properties at ambient temperature
Sandvik grade* Yield strength
ksi
0.2% offset
Tensile
strength
min ksi
Elongation
min %
Hardness
HRC
max
SAF 2205™ / 22Cr 75–100 95 25 28
130–160 140 10 36
SAF 2507® / 25Cr ≥80 116 25 32
SAF 3207 HD™ ≥112 ≥138 15 36
Sanicro® 28 110–140 115 12 32
125–145 130 10 35
Sanicro® 29 110-140 115 12 35
125-145 130 10 37
Sanicro® 48 110-140 115 11 35
125-150 130 10 37


*All grades are included in NACE MR 0175 and ISO 15156.

Production tubing is supplied in outside diameters up to and including 7 3/4".

Other sizes are available on request for Mother tubes for Couplings, x-overs and other accessories.