Socket welding fittings according to ANSI/ASME

Tube, pipe, fittings and flanges

Alleima holds a large stock of stainless, forged, socket welding fittings in F304/304L and F316/316L (dual marked and certified). Our socket welding fittings are according to ASTM A182, ASME B16.11. Socket weld unions are according to MSS SP-83.

ASME 3000 lbs forged, socket weld fittings from Alleima are white pickled with hardness according to NACE MR0175, IC according to ASTM A262E and PMI tested.

Alleima socket weld fittings are certified according to EN 10204/3.1.

Types of socket welding fittings