Tees, socket weld

Tube, pipe, fittings and flanges

ASTM A182 3000 lbs ASME B16.11 / BS 3799

Product code example:

FST-316L-1-3000

● = stock standard

3707-[Converted].png
Nominal pipe size B L1 C G D A
Weight
ASTM
ASTM
in. mm socket mm mm mm mm ~kg/pce 304/304L 316/316L
1/4
3/8
1/2
3/4
14.20
17.60
21.80
27.20
9.53
9.53
9.53
12.50
3.30
3.51
4.09
4.27
3.02
3.20
3.73
3.91
8.86
12.14
15.42
20.55
11.11
13.49
15.88
19.05
0.11
0.16
0.34
0.41






1


2
33.90
42.70
48.80
61.20
12.50
12.50
12.50
16.00
4.98
5.28
5.54
6.05
4.55
4.85
5.08
5.54
26.26
34.67
40.51
52.12
22.23
26.99
31.75
38.10
0.65
0.95
1.33
2.20