Superheater tubes and reheater tubes

Tube, pipe, fittings and flanges

Superheater tubes and reheater tubes in a comprehensive range of stainless steels and nickel alloys covering outside diameters 12 to 260 mm (0.472 to 10.24 in.).

Superheater tubes and reheater tubes

Our superheater tube and reheater tube materials cover all types of fuel, such as coal, gas, oil, black liquor and biomass. The Alleima portfolio also includes composite tubes consisting of two different alloys fully bonded together.

Increased efficiency in coal-fired power boilers

Our new material Sanicro® 25 is engineered for the next generation of coal-fired power boilers, contributing to significantly greater efficiency and sharply lower CO2 emissions. It is ideal for superheater and reheater tubes, allowing for material temperatures of up to 700ºC (1290ºF). Read more about Sanicro® 25.

Below are the most typical applications for superheater and reheater tubes. Contact us for advice on product selection or other technical support.

Product standards
Alleima grade Typical applications
Sanicro® 25
(UNS S31035)
Superheater and reheater tubes in the next generation of coal-fired power boilers for material temperatures of up to 700ºC (1290ºF).
Sanicro® 31HT
(UNS N08811/N08810)
Superheater and reheater tubes in boilers with corrosive conditions.
Sanicro® 41
(UNS N08825)
Superheater and reheater tubes in boilers with corrosive conditions. Sanicro® 41 is generally more resistant to flue gases compared to Sanicro 31HT.
Sanicro® 28
(UNS 08028, EN 1.4563)
Radiant syngas coolers in IGCC gasification.
Superheater tubes in boilers with corrosive conditions. The high chromium content of Sanicro® 28 contributes to high gas corrosion resistance.
Sanicro® 30
(UNS N08800)
Radiant syngas coolers in IGCC gasification.
Esshete 1250
(EN 1.4982)
Superheater and reheater tubes in sub-critical and supercritical coal-fired, biomass and other boilers. Esshete 1250 has higher creep strength than most other alloys.
Alleima 7RE10
(UNS S31008/S31009)
Superheater tubes in boilers with corrosive conditions.
Alleima 3R69 BT**
(EN 1.4910)
Superheater and reheater tubes in sub-critical and supercritical coal-fired boilers.
Alleima 8R61
(EN 1.4918)
Superheater and reheater tubes in sub-critical coal-fired boilers and other boilers.
Alleima 6LR62
(UNS S31600/S31609)
Superheater and reheater tubes in sub-critical coal-fired boilers and other boilers.
Alleima 8R41
(EN 1.4961)
Superheater and reheater tubes in sub-critical coal-fired boilers and other boilers.
Alleima 8R40
(UNS S34709, ASTM 347H)
Superheater and reheater tubes in sub-critical coal-fired, biomass and other boilers. Sandvik 8R40 can also be supplied in a fine-grain version.
Alleima 6R44
(UNS S34709, ASTM 347H)
Superheater and reheater tubes in sub-critical coal-fired, biomass and other boilers.
Alleima 6R35
(UNS S32109, ASTM 321H)
Superheater and reheater tubes in sub-critical coal-fired boilers and other boilers.
Alleima 5R10
(UNS S30409, ASTM 304H)
Superheater and reheater tubes in sub-critical coal-fired boilers and other boilers.

*Esshete 1250 is a trademark owned by Corus