Titanium tubing

Titanium tubing tubing suitable for environments and applications where the properties of stainless steels are not sufficient.

Vill du veta mer?

Ring oss Mejla oss

Typical applications include tubing for the aerospace industry and heat-exchangers.

Sandvik titanium tubing is available in size range outside diameter 9.53–38.1 mm (3/8–1½ in.) with wall thicknesses from 0.7 to 5 mm (0.0275 to 0.1968 in.). The titanium tubes tubes are delivered in straight lengths or as U-bent tubes.

Grades and standards

Titanium tube grades (other grades are available on request)
Sandvik grade UNS ASTM/ASME W.Nr. AFNOR
Ti Grade 1 (CP Ti) R50250 Grade 1 W.Nr. 3.7025 T-35
Ti Grade 2 (CP Ti) R50400 Grade 2 W.Nr. 3.7035 T-40
Ti Grade 3 (CP Ti) R50550 Grade 3 W.Nr. 3.7055 T-50
Ti Grade 7 R52400 Grade 7 W.Nr. 3.7235 -
Ti Grade 9 R56320 Grade 9 W.Nr. 3.7195 T-A3V2.5
Ti Grade 11 R52250 Grade 11 W.Nr. 3.7225 -
Ti Grade 12 R53400 Grade 12 W.Nr. 3.7105 -
Ti Grade 16 R52402 Grade 16 - -
Ti Grade 17 R52252 Grade 17 - -
Ti Grade 26 R52404 Grade 26 - -
Ti Grade 28 R52254 Grade 28 - -
Sandvik grade Description
Ti Grade 1 (CP Ti) Relatively low-strength and high-ductility pure titanium (Cp).
Ti Grade 2 (CP Ti) Medium-strength pure titanium (Cp).
Ti Grade 3 (CP Ti) High strength pure titanium (Cp).
Ti Grade 7 Medium-strength Pd-alloyed titanium for enhanced corrosion properties.
Ti Grade 9 High-strength titanium alloyed with 3% Al and 2.5% V.
Ti Grade 11 Low-strength titanium plus 0.12-0.25% Pd for enhanced corrosion properties.
Ti Grade 12 High-strength titanium alloy plus 0.3% Mo and 0.8% Ni for enhanced corrosion properties.
Ti Grade 16 Medium-strength titanium plus 0.04-0.08% Pd for enhanced corrosion properties.
Ti Grade 17 Low-strength titanium plus 0.04-0.08% Pd for enhanced corrosion properties.
Ti Grade 26 Medium-strength titanium plus 0.08-0.14% Ru for enhanced corrosion properties.
Ti Grade 28 High-strength titanium alloy plus 3% Al, 2.5% V and 0.08%-0.14% Ru for enhanced corrosion properties.
Type of product Grade(s) Technical requirements*
according to
Titanium tubes and pipes Ti and Ti alloy grades 1, 2, 3, 7, 9, 11, 12, 16, 17, 26 and 28 ASTM B337, ASTM B338, ASME SB338
NACE MRO 175-94
VdTÜV 230/2
Dimensional tolerances acc. to DIN 17861 D3/T3 or closer

*Other requirements on request

Mechanical properties

Sandvik gradeUNSProof strength
Rp0.2 MPa min
Tensile strength
Rm MPa min
Elongation
A % min
Cp Ti Grade 1 R50250 138-310 240 24
Cp Ti Grade 2 R50400 275-450 345 20
Cp Ti Grade 3 R50550 380-550 450 18
Ti Grade 7 R52400 275-450 345 20
Ti Grade 9 R56320 483 620 15
Ti Grade 11 R52250 138-310 240 24
Ti Grade 12 R53400 345 483 18
Ti Grade 16 R52402 275-450 345 20
Ti Grade 17 R52252 138-310 240 24
Ti Grade 26 R52404 275-450 345 20
Ti Grade 28 R52254 483 620 15

Sizes and tolerances

Sizes and tolerances for titanium tubes

Sandvik titanium tubes are available in size range outside diameter 9.53-38.1 mm (3/8 - 1 1/2 in.) with wall thicknesses from 0.7 to 5 mm (0.0275 to 0.1968 in.)*.

OD = outside diameter
WT = wall thickness

Size OD, mm (in.)Tolerances OD, mm (in.)WT min wall %
< 25.4 (< 3/8) ±0.102 (0.004) +20/-0
25.4-38.1 (1-1 1/2) ±0.127 (0.005) +20/-0

Tolerances for OD < 15.9 or > 38.1 - or closer tolerances - after special agreement.

*Limitations for some ratios of OD/WT exist

Standards
Type of productGrade(s)Technical requirements
Titanium tubes and pipes Ti and Ti alloy grades: 1, 2, 3, 7, 9, 11, 12, 16, 17, 26, 28 and 29 ASTM B337, ASTM B338, ASME SB338
NACE MRO 175-94
VdTÜV 230/2
Dimensional tolerances acc. to DIN 17861 D3/T3 or closer

Lengths

Titanium tubes are delivered in straight lengths up to 16.5 meters (54 ft). U-bent tubes are available on request.