Sandvik SanRig 80 stainless rig rod

Sandvik wire products acquired by Zapp AG

Sandvik’s round and flat wire business has been acquired by Zapp AG from August 31, 2018. Over the coming months Zapp will be integrating the Sandvik portfolio, to provide a smooth transition for customers. During the integration period, the full line of Sandvik wire products will continue to be accessible on this website, or via the Zapp website.

Please note: divestment of round and flat wire products does not include EXERA fine wire and medical wire components manufactured by Sandvik Palm Coast.

ZAPP WEBSITE

Stainless steel rig rod for rigging on sailing boats and yachts that meets the high demands on tensile strength, toughness and corrosion resistance in marine environments. Sandvik SanRig 80 stainless rig rod is also used for a range of applications within the architectural area and building construction.

Vill du veta mer?

Ring oss Mejla oss

Stainless rig rod in coils

Sandvik SanRig 80 stainless steel rig rod in coils is available in size range 4–17.9 mm (0.157–0.70 in.). It is delivered in coils of 150-250 kg (330-550 lbs), depending on size.

Stainless rig rod as bar

Sandvik SanRig 80 stainless steel rig rod can be delivered as bar in straight lengths in size range 16.8–50.8 mm (0.63–2.0 in.). It can be supplied in the unpolished or fully polished condition.

Sandvik SanRig 80 rig rod can be supplied from stock for immediate repair and service type installations, but can also be made to order for specific projects such as new yacht builds and scheduled refurbishment work. Contact us for stock list.

Sandvik SanRig 80 (UNS S31675) stainless steel rig rod is comparable to grade Nitronic* 50.

Chemical composition (nominal), %
C
max.
Si Mn P
max.
S
max.
Cr Ni Mo N Nb
0.005 0.5 4.0 0.020 0.015 20.5 10 2.4 0.4 0.3
Sizes and properties for Sandvik SanRig 80 rig rod
Diameter, mm (in.) Form of supply
Weight, kg/m
Breaking load min (lbf)
4.50 (0.17) Coil
0.12
4955
5.50 (0.20) Coil
0.16
6399
5.70 (0.22) Coil
0.20
8316
6.40 (0.25) Coil
0.25
10484
7.10 (0.28) Coil
0.31
12903
7.50 (0.30) Coil
0.35
14398
8.40 (0.33) Coil
0.44
18061
9.50 (0.37) Coil
0.57
23101
11.10 (0.44) Coil
0.77
30450
12.70 (0.45) Coil
1.00
39861
14.30 (0.56) Coil
1.28
48733
16.80 (0.66) Coil
1.77
62297
16.80 (0.66) Bar 1.77 62000
17.90 (0.71) Coil
1.98
76358
17.90 (0.71) Bar 1.98 76000
19.50 (0.77) Bar 2.35 91000
22.20 (0.87) Bar 3.05 115000
25.40 (1.00) Bar 3.99 150000
27.10 (1.07) Bar 4.54 170000
28.60 (1.13) Bar 5.06 195000
30.30 (1.19) Bar 5.67 220000
33.40 (1.31) Bar 6.90 260000
38.10 (1.50) Bar 8.97 320000
41.28 (1.63) Bar 10.53 360000
44.45 (1.75) Bar 12.21 430000
50.80 (2.00) Bar 15.95 540000

* Nitronic is a registered trademark owned by AK Steel Corporation, US