Hot isostatic pressed (HIP) products数据表

数据表已更新2019-12-17 08:02 (取代之前所有版本)

免责声明:建议仅供参考,针对特定应用场合的焊材适用性我们需要了解实际服役条件后才能予以确认。因持续研发导致的产品技术数据更改不会另行通知。该数据表仅适用于山特维克焊材。

APM 2377 is a powder metallurgical duplex (austenitic-ferritic) stainless steel manufactured by Hot Isostatic Pressing (HIP). It is characterized by high strength and good corrosion resistance. Applications include for example offshore components.

Standards

  • UNS: S31803, S32205
  • EN Number: 1.4462

Approvals

  • NACE MR0175/ISO 15156
  • ASME B31.3
  • APM 2377 supplied by Sandvik is qualified according to NORSOK M650 D44