Ferritic stainless steel metal powder

Sandvik's standard range of Osprey™ ferritic stainless steel metal powder includes grades of ASTM 430 and 434 types. The ferritic stainless steel metal powder is used in processes, such as:

Chcete vědět víc?

Zavolejte nám Zašlete nám e-mail

Selected ferritic stainless steels incl. chemical composition (nominal), %
Alloy (UNS) Description Fe C Cr Si Mn S P
430
(S43000)
General purpose ferritic steel Bal. 0.12 16.0-18.0 1.0 1.0 0.03 0.04
430L Ferritic soft-magnetic stainless steel Bal. 0.03 16.0-18.0 1.0 1.0 0.03 0.04
434
(S43400)
Molybdenum-alloyed ferritic steel
for improved corrosion resistance
in automotive trim
Bal. 0.12 16.0-18.0 1.0 1.0 0.03 0.04

Other ferritic stainless steels are also available. Contact us to discuss Sandvik's full range of metal powder alloys.