Ammonium hydroxide

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Ammonium perchlorate

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Ammonium sulphide

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Antimony chloride

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Barium nitrate

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Beryllium chloride

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Butyl acetate

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Butyl alcohol

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Calcium arsenate

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Calcium hydroxide + calcium chloride

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and