Bond E1

Wire insulations and coatingsDatablad

Datablad opdateret 2019-09-06 07:07 (afløser alle tidligere versioner)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Bond E1 is a thermoplastic modified epoxy bondcoat. It will soften and reflow with the application of heat during or after coil winding.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.