Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 2C48 is a ferritic, heat resisting, stainless chromium steel, characterized by:

  • Good resistance to reducing sulphurous gases
  • Very good resistance to oxidation in air
  • good resistance to oil-ash corrosion
  • Resistance to molten copper, lead and tin

This steel can be used at temperatures up to 1075°C (1970°F). However, allowance should be made for the low creep strength at the highest temperatures in order to avoid distortion due to the mass of the steel.

Standards

  • : 446-2
  • : S44600

Product standards

  • ASTM A268

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.