Pipe in sizes according to ANSI/ASME

Seamless, stainless pipe in sizes according to ANSI/ASME. Our ANSI/ASME stainless steel pipe is delivered in random lengths or cut to fixed lengths.
Vil du vide mere?
Materials
The Sandvik program of ANSI/ASME seamless pipe includes austenitic stainless steels, duplex and super-duplex stainless steels and a high-alloy austenitic stainless steel.
List of materials
Sandvik grade | UNS | ASTM | EN no. |
---|---|---|---|
Sandvik 3R12 | S30403 / S30400 | 304L / 304 | 1.4306 / 1.4301 |
Sandvik 3R65 | S31603 / S31600 | 316L / 316 | 1.4404 / 1.4401 |
SAF 2205™ | S31803 / S32205 | - | 1.4462 |
SAF 2507® | S32750 | - | 1.4410 |
Sandvik 2RK65 | N08904 | - | 1.4539 |
Sandvik 254 SMO | S31254 | - | 1.4547 |
Available online
This product can be ordered online via our self-service platform E-Track, where you can also see stocks, get prices and view your order history.
E-Track is currently available in selected European countries but we are working on expanding the availability.
Stock program
Pipe is stocked according to ANSI/ASME B36.19.
OD = outside diameter, WT = wall thickness.
Stock standard items: C = Central warehouse (Europe), U = United States
OD mm |
WT mm |
in. | Sch | Kg/m | Sandvik 3R12 |
Sandvik 3R65 |
Sandvik SAF 2205 |
Sandvik SAF 2507 |
Sandvik 2RK65 |
Sandvik 254 SMO |
---|---|---|---|---|---|---|---|---|---|---|
13.72 | 1.65 | 1/4 | 10S | 0.50 |
C
|
C
|
- | - | - | - |
13.72 | 2.24 | 1/4 | 40S | 0.64 |
C
|
C
|
- | - | - | - |
13.72 | 3.02 | 1/4 | 80S | 0.81 |
C
|
C
|
- | - | - | - |
17.15 | 1.65 | 3/8 | 10S | 0.64 |
C
|
C
|
- | - | - | - |
17.15 | 2.31 | 3/8 | 40S | 0.86 |
C
|
C
|
- | - | - | - |
17.15 | 3.20 | 3/8 | 80S | 1.12 |
C
|
C
|
- | - | - | - |
21.34 | 2.11 | 1/2 | 10S | 1.02 |
C
|
C
|
- |
C
|
C1)
|
-
|
21.34 | 2.77 | 1/2 | 40S | 1.29 |
C, U
|
C, U
|
C
|
C
|
C1)
|
C
|
21.34 | 3.73 | 1/2 | 80S | 1.65 |
C, U
|
C, U
|
C
|
- | - | - |
26.67 | 2.11 | 3/4 | 10S | 1.30 |
C
|
C
|
C
|
- |
C1)
|
-
|
26.67 | 2.87 | 3/4 | 40S | 1.71 |
C, U
|
C, U
|
C
|
C
|
-
|
C
|
26.67 | 3.91 | 3/4 | 80S | 2.23 |
C, U
|
C, U
|
C
|
- | - | |
33.40 | 2.77 | 1 | 10S | 2.13 |
C, U
|
C, U
|
C
|
C
|
C1)
|
C
|
33.40 | 3.38 | 1 | 40S | 2.54 |
C, U
|
C, U
|
C
|
C
|
C1)
|
C
|
33.40 | 4.55 | 1 | 80S | 3.29 |
C, U
|
C, U
|
C
|
C
|
- | - |
33.40 | 6.352) | 1 | 160 | 4.30 |
C, U
|
C, U
|
- | - | - | - |
42.16 | 2.77 | 1¼ | 10S | 2.73 |
C
|
C
|
C
|
C
|
C1)
|
-
|
42.16 | 3.56 | 1¼ | 40S | 3.44 |
C, U
|
C, U
|
C
|
- |
C1)
|
-
|
42.16 | 4.85 | 1¼ | 80S | 4.53 |
C, U
|
C
|
- | - | - | - |
42.16 | 6.352) | 1¼ | 160 | 5.69 |
C, U
|
C
|
- | - | - | - |
48.26 | 2.77 | 1½ | 10S | 3.16 |
C, U
|
C, U
|
C
|
C
|
C | C |
48.26 | 3.68 | 1½ | 40S | 4.11 |
C, U
|
C, U
|
C
|
C, U
|
C
|
C
|
48.26 | 5.08 | 1½ | 80S | 5.49 |
C, U
|
C, U
|
C
|
C
|
- | - |
60.33 | 2.77 | 2 | 10S | 3.99 |
C, U
|
C, U
|
C
|
C
|
-
|
C
|
60.33 | 3.91 | 2 | 40S | 5.52 |
C, U
|
C, U
|
C
|
C, U
|
C
|
C
|
60.33 | 5.54 | 2 | 80S | 7.60 |
C, U
|
C, U
|
C
|
C
|
- | C |
60.33 | 8.742) | 2 | 160 | 11.29 |
C, U
|
C, U
|
C
|
- | - | - |
73.03 | 3.05 | 2½ | 10S | 5.35 |
C, U
|
C
|
C
|
- |
C
|
-
|
73.03 | 5.16 | 2½ | 40S | 8.77 |
C, U
|
C, U
|
C
|
- |
C
|
-
|
73.03 | 7.01 | 2½ | 80S | 11.59 |
C, U
|
C, U
|
C
|
- | - | - |
88.90 | 3.05 | 3 | 10S | 6.56 |
C, U
|
C, U
|
C
|
C
|
C
|
C
|
88.90 | 5.49 | 3 | 40S | 11.47 |
C, U
|
C, U
|
C
|
C, U
|
C
|
C
|
88.90 | 7.62 | 3 | 80S | 15.51 |
C, U
|
C, U
|
C
|
- | - | C |
88.90 | 11.132) | 3 | 160 | 21.67 |
C
|
C, U
|
C
|
- | - | - |
101.60 | 3.05 | 3½ | 10S | 7.53 |
C
|
C
|
- | - | - | - |
101.60 | 5.74 | 3½ | 40S | 13.78 |
C, U
|
C
|
- | - | - | - |
101.60 | 8.08 | 3½ | 80S | 18.92 |
C, U
|
C, U
|
- | - | - | - |
114.30 | 3.05 | 4 | 10S | 8.50 |
C, U
|
C, U
|
C
|
C
|
- | C |
114.30 | 6.02 | 4 | 40S | 16.32 |
C, U
|
C, U
|
C
|
C
|
C
|
C
|
114.30 | 8.56 | 4 | 80S | 22.67 |
C, U
|
C, U
|
C
|
-
|
- | C |
114.30 | 13.492) | 4 | 160 | 34.05 |
C, U
|
C
|
C
|
- | - | - |
141.30 | 6.55 | 5 | 40S | 22.10 |
C, U
|
C
|
- | - | - | - |
141.30 | 9.53 | 5 | 80S | 31.44 |
C, U
|
C
|
- | - | - | - |
141.30 | 15.882) | 5 | 160 | 49.87 |
C
|
C
|
- | - | - | - |
168.28 | 3.4 | 6 | 10S | 14.04 |
C, U
|
C, U
|
- | - | - | - |
168.28 | 7.11 | 6 | 40S | 28.69 |
C, U
|
C, U
|
C
|
C
|
- | - |
168.28 | 10.97 | 6 | 80S | 43.21 |
C, U
|
C, U
|
- | - | - | C |
168.28 | 14.27 | 6 | 120 | 54.75 | - | - |
C
|
- | - | - |
168.28 | 18.262) | 6 | 160 | 68.59 |
C
|
C
|
C
|
- | - | - |
219.08 | 8.18 | 8 | 40S | 43.20 |
C, U
|
C
|
C
|
C
|
- | - |
219.08 | 12.7 | 8 | 80S | 65.63 |
C
|
C
|
- | - | - | - |
219.08 | 18.23 | 8 | 120 | 91.30 | - | - |
C
|
- | - | - |
219.08 | 23.012) | 8 | 160 | 112.97 |
C
|
C
|
C
|
- | - | - |
1) Tested acc. to ASTM A312 and AD2000-W2 Einbaurohre TÜV Bl. 421 incl. hot tensile test at +400ºC (752ºF).
2) ASME B36.10
Tolerances
For ASTM A312 and ASTM A790, acc. to ASTM A999
Size, mm | Tolerance OD, mm |
---|---|
13.72-48.3 | +0.4/-0.8 |
>48.3-114.3 | +/- 0.8 |
>114.3-219.1 | +1.6/-0.8 |
Tolerances on wall thickness
Size, mm | Wall thickness, % | WT/OD ratio |
---|---|---|
13.72-73.03 | +20/-12.5 | All |
88.90-219.10 | +22.5/-12.5 | Less or equal to 0.05 |
88.90-219.10 | +15/-12.5 | Above 0.05 |
Product standards
Sandvik 3R12 (ASTM 304L), Sandvik 3R65 and 3R60 (ASTM 316L)
- ASTM A312 incl. corrosion test acc. to ASTM A262 Pr.E.
- NACE MR-0.175/ISO 15156
- Tolerances and leak test acc. to ASTM A312/A999
- NORSOK MDS-S01 (ASTM 316L)
SAF 2205™ (UNS S31803/S32205) and SAF 2507® (UNS S32750)
- ASTM A790 incl. corrosion test acc. to ASTM G-48 Method A (SAF 2205 at 25ºC/77ºF, SAF 2507 at 50ºC/122ºF - both for 24 hours).
- NORSOK MDS D-41 (SAF 2205)
- NORSOK MDS D-51 (SAF 2507)
Sandvik 2RK65™ (UNS N08904)
ASTM A312. Sizes marked 2) are also tested acc. to AD2000-W2 Einbaurohre TÜV Bl. 421 incl. hot tensile test at +400ºC (752ºF).
Sandvik 254 SMO (UNS S31254)
- ANSI B36.19
- ASTM A-312, ASME SA-312
- PED 2014/68/EU, EN 10216-5 TC1
- NORSOK M-630 ED-6, NORSOK MDS R11 REV.5
- IOGP S-563 DEC.2018, MDS IR111/ IR111S REV.01
- NACE MR0175/ ISO 15156-3, NACE MR0103/ISO 17945-1