Tube, pipe, fittings and flanges
Seamless high-pressure tubes for a variety of high-pressure applications using liquid or gas as the pressure medium, such as hydraulic installations, test benches and water-jet cutting equipment.
High-pressure tubes from Alleima are characterized by high yield strength and high tensile strength in combination with high elongation. The pressure resistance is guaranteed by the very smooth inside surface. An autofrettage treatment prolongs the cycle fatigue behavior.
Alleima grade | UNS | ASTM | EN steel no. | W.Nr. | AFNOR |
---|---|---|---|---|---|
Alleima® 5R10 | S30400 | 304 | 1.4301 | 1.4301 | Z2CND18-09 |
Alleima® 3R65 | S31603/S31600 | 316L/316 | 1.4404/1.4401 | 1.4404 | Z2CND17-12 |
SAF™ 2507 | S32750 |
-
|
1.4410 |
-
|
-
|
Alleima HP160* |
-
|
-
|
-
|
-
|
-
|
Alleima® 254 SMO | S31254 | - | - | - | Z1CNDU20-18-06AZ |
* Contact us for more information
Alleima grade | Yield strength Rp0,2 min. MPa |
Tensile strength Rm min. MPa |
Elongation A %, min |
---|---|---|---|
Alleima® 5R10 1) | 600 | 700 | 18 |
Alleima® 3R65 1) | 600 | 700 | 18 |
SAF™ 2507 2) | 550 | 800-1,000 | 25 |
Alleima HP160* 2) | 450 | 850 | 35 |
Alleima® 254 SMO 2) | 340 | 650 | 65 |
1) Hard condition.
2) Annealed condition. Tubes with higher values can be offered on request.
* Contact us for more information
Alleima high-pressure tubes are manufactured in standard sizes according to the table. Standard lengths are 4-7 meters. Other sizes and lengths up to 16 meters can be offered on request.
OD | = Outside diameter |
ID | = Inside diameter |
WT | = Wall thickness |
OD mm |
OD in. |
ID mm |
ID in. |
WT mm |
WT in. |
Working pressure
(stat.)1) bar Alleima® 3R65/5R10 |
Working pressure
(stat.) bar Alleima® HP160 |
Weight kg/m |
---|---|---|---|---|---|---|---|---|
6
|
-
|
2.2
|
-
|
1.90
|
3,120
|
5,710
|
0.195
|
|
6.35
|
1/4
|
2.39
|
3/32
|
1.98
|
0.0781
|
3,045
|
5,580
|
0.217
|
6.35
|
1/4
|
2.29
|
0.0902
|
2.03
|
0.0799
|
3,180
|
-
|
0.220
|
6.35
|
1/4
|
1.59
|
1/16
|
2.38
|
0.0938
|
4,300
|
7,890
|
0.237
|
9.52
|
3/8
|
3.20
|
1/8
|
3.16
|
0.1245
|
3,380
|
6,190
|
0.503
|
9.52
|
3/8
|
1.60
|
1/16
|
3.96
|
0.1560
|
5,530
|
10,140
|
0.551
|
14.00
|
-
|
8.00
|
-
|
3.00
|
-
|
2,330
|
-
|
0.826
|
14.00
|
-
|
5.00
|
-
|
4.50
|
-
|
3,200
|
-
|
1.070
|
14.30
|
9/16
|
8.00
|
5/16
|
3.15
|
0.1240
|
2,380
|
4,360
|
0.879
|
14.30
|
9/16
|
4.76
|
3/16
|
4.77
|
0.1878
|
3,390
|
6,210
|
1.138
|
19.05
|
3/4
|
1.80
|
-
|
8.63
|
-
|
-
|
12,00
|
2.251
|
30.00
|
-
|
10
|
-
|
10
|
-
|
-
|
6,250
|
5.008
|
1) Calculation basis:
K: Factor = OD/ID
K < 2: Calculation according to AD-regulation B10
K > 2: Calculation basis full plastic condition. Safety factor 0.45.
OD and ID: +/- 0.1 mm
WT: +/- 10%
Other tolerances can be offered on request.
As a standard, the internal surface is free from laps, flaws and fissures deeper than 0.1 mm, max. 5 defects > 0.05 mm per cross-section. On prior consultation, depth of defects of max. 0.02 mm according to DIN ISO 8535-1 can be reached.
Testing of high-pressure tubes includes:
Tests made on request are, for example:
The tests carried out are certified according to DIN EN 10204 3.1. Reception tests according to DIN EN 10204 3.2 by neutral experts can be made on request.
Examinations to determine the cycle fatigue behavior under defined operating conditions can be carried out on request. We offer individual advice.
Our testing laboratory for high-pressure tubes is accredited according to ISO 17025.
The scope of inspection depends on the customer specification.