191 hits
Safurex® Product form:Tube and pipe, seamless
Standard:UNS S32906 | EN number 1.4477
Safurex® is a high-alloy duplex (austenitic-ferritic) stainless steel developed to withstand the corrosive environments present in the Stamicarbon urea process. The grade is characterized by:
Standard:
A hardenable, free-cutting carbon steel characterized by excellent machinability. It has high hardness, high wear resistance and exceptional dimensional stability after hardening.
Standard:UNS S31600/ S31603 | ASTM 316/316L | EN number 1.4401/1.4404
Austenitic stainless steel alloyed with molybdenum. The grades are part of the Exera® medical materials range.
Standard:ASTM 302/302VM, '304V' | EN number 1.4310 NS
Austenitic stainless steels with moderate tensile strength, good corrosion resistance and moderate fatigue and relaxation resistance. Exera® 12R10 HV is vacuum remelted for higher cleanliness. The grades are part of the Exera® medical materials range.
Standard:
Composite wire consisting of a Exera® F562 CoCrMo alloy shell and a secondary alloy as the core material.
Standard:UNS S32205/S31803 | EN number 1.4462
A duplex (austenitic-ferritic) stainless steel characterized by high tensile strength and very good relaxation resistance combined with high resistance to fatigue and corrosion. The grade is part of the Exera® medical materials range.
Standard:UNS S30151 | EN number 1.4310
A molybdenum-alloyed austenitic stainless steel characterized by high tensile strength and high corrosion, fatigue and relaxation resistance. Exera® 11R51 HV is vacuum remelted for higher cleanliness. Both versions are part of the Exera® medical wire portfolio.
Sandvik 6R35 (Several product forms available)
UNS s32100, S32100, S32109 | ASTM 321/321H, TP321, TP321H | EN number 1.4541, 1.4940
A titanium-stabilized austenitic stainless steel.
Sandvik 5R75 (Several product forms available)
UNS S31635 | ASTM 316Ti, TP316Ti | EN number 1.4571
A titanium-stabilized austenitic stainless steel alloyed with molybdenum.
Standard:UNS S31254 | EN number 1.4547
A high-alloy austenitic stainless steel characterized by very high resistance to corrosion in chloride media and good mechanical strength.