Precision tubes

Stainless steel precision tubes available as thin wall tubes in seamless or welded redrawn condition or as seamless thick wall tubes. Our precision tube program covers a wide range of materials, such as:
- Austenitic stainless steels
- Duplex stainless steels
- Nickel alloys
Sandvik's precision tubes are delivered with cold drawn, ground, extremely polished or bright surface, depending on size and wall thickness.
Outside diameter | 0.5-50.8 mm (0.0197-2 in.) |
---|---|
Wall thickness | 0.10-3 mm (0.0039-0.118 in.) |
Go to thin wall precision tubes
Outside diameter | 0.787-130 mm (0.031-5 in.) |
---|---|
Wall thickness | 0.254-19.05 mm (0.010-0.750 in.) |