Lime kiln lances

Sandvik provides stainless steel tubes for lime kiln lances. Sandvik lance tubes provide long service life and reduced maintenance costs, particularly under the severe high-temperature corrosion conditions encountered in lime kilns. Sandvik stainless steel lance tubes are therefore a cost-effective alternative to lance tubes in conventional grades of, for example, ASTM 310H and 316H types.

Our program also includes welding products.

Lance tube materials (other grades can be offered on request)
Sandvik grade
(UNS)
Description
Sandvik 253 MA*
(UNS S30815)

Austenitic stainless steel alloyed with nitrogen and REM (rare earth metals). A multi-purpose grade suitable for temperatures from 600 to 1000ºC (1112 to 1832ºF).

Sandvik 353 MA*
(UNS S35315)

Austenitic stainless steel alloyed with nitrogen and REM (rare earth metals). Suitable for oxidizing, carburizing and nitriding conditions. Suitable for temperatures from 800 to 1150ºC (1472 to 2102ºF).

Sandvik 4C54**
(UNS S44600)

Ferritic stainless steel with a high chromium content (26.5%) suitable for sulphudizing conditions. Suitable for temperatures from 600 to 1000ºC (1112 to 1832ºF).

* 253 MA and 353 MA are trademarks owned by Outokumpu OY.
** Sandvik 4C54 performs well also under sulphidizing conditions.