Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sanmac 4571 is a titanium-stabilized, molybdenum-alloyed austenitic chromium-nickel steel with improved machinability.

Standards

  • ASTM: 316Ti
  • UNS: S31635
  • EN Number: 1.4571
  • W.Nr.: 1.4571

Product standard

  • EN 10088-3, EN 10088-5 (dimensions up to 250 mm)
  • EN 10272, EN 10222-5, (dimensions ≥ 180 mm), AD-2000-W2
  • ASTM A479, ASTM A276
  • Chemical composition and mechanical properties acc. to ASTM A182

Approvals

  • TÜV AD Merkblatt W0/TRD 100
  • Pressure Equipment Directive (2014/68/EU)
  • Pre-approval for PMA

Certificate

Status according to EN 10 204/3.1

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.