Sandvik 3R60™

BilletsDatasheet

Datasheet updated 2020-12-10 07:47 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 3R60™ is an austenitic chromium-nickel steel with minimum 2.5% molybdenum and a low carbon content.

Sandvik 3R60™ is also supplied in a variant for the urea industry, Sandvik 3R60™ Urea Grade.

Standards

  • ASTM: 316L
  • UNS: S31603, S31600
  • EN Number: 1.4435, 1.4436
  • W.Nr.: 1.4435, 1.4436
  • SS: 2353, 2343
  • AFNOR: Z3CND18-14-03
  • BS: 316S13

Product standards

  • EN 10088-3
  • ASTM A-314

Suitable for production of flanges etc. according to ASTM A-182

Certificates

Status according to EN 10 204 3.1

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.