Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 3R65 is a molybdenum-alloyed austenitic chromium-nickel steel with a low carbon content.

Standards

  • ASTM: 316L, 316
  • UNS: S31603, S31600
  • W.Nr.: 1.4404, 1.4401
  • SS: 2348
  • BS: 316S11

Product standards

  • EN 10088-3
  • ASTM A-314

Suitable for production of flanges etc. according to ASTM A-182

Certificates

Status according to EN 10 204 3.1

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.