Sandvik 22.8.3.L

Welding strip Datasheet

Datasheet updated 2018-07-20 15:06 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 22.8.3.L is a strip electrodes used to obtain a 2209 (SAF 2205) corrosion resistant overlay weld deposit on carbon, carbon-manganese and low-alloy steels using submerged-arc welding (SAW) with Sandvik 10SW flux or electroslag welding (ESW) with Sandvik 47S flux. Other combinations and conditions are possible.

Standards

  • ISO 14343: 22 9 3 N L
  • AWS A5.9/ASME SFA5.9: EQ2209

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.