Alleima® 2RE10 is a high-alloy austenitic stainless steel, developed specifically for demanding applications in the nitric acid industry. The grade is gaining a good reputation for resisting corrosion at high temperatures, thereby extending the lifetime of process equipment.

Alleima® 2RE10 is especially well suited for the tubing used in condenser-coolers where re-boiling can accelerate corrosion rates. It is highly resistant to corrosion, with extremely low carbon and impurity levels and is available in outer diameters up to 80 mm (3.15 in).

Material datasheet

Material datasheet for Alleima® 2RE10