Outlets, socket welding

Need to know more?

Call us Email us

ASTM A182 3000 lbs MSS SP-97

Note: final adjustment on run pipe sizes to be made on site.

(Generally the outlets are stocked with 1/4-1 in. larger run pipe sizes).

Product code example:

FSOR-316L-1-3000

● = stock standard

Branch
Weight
ASTM
ASTM
Size D1, in. ~kg/pce 304/304L 316/316L
1/2
3/4
1
0.13
0.24
0.37




1 ½
2
0.65
1.02