Hexagon head males, NPT-threaded

ASTM A182 3000 lbs, ASME B16.11 / BS 3799
6000 lbs (=3000 lbs)
Product code example:
FTHHP-316L-1/4-6000
● = stock standard
Nominal pipe size | B | N | C | Weight | ASTM | ASTM |
---|---|---|---|---|---|---|
in. | mm (min.) | mm | mm | ~kg/pce | 304/304L | 316/316L |
1/4
3/8 1/2
3/4 |
11.0
13.0 14.0 16.0 |
16.0
19.0 22.0 27.0 |
6.0
8.0 8.0 10.0 |
0.03
0.05 0.08 0.15 |
●
● ● ● |
●
● ● ● |
1
1 ¼ 1 ½ 2 |
19.0
21.0 21.0 22.0 |
35.0
45.0 51.0 64.0 |
10.0
14.0 16.0 18.0 |
0.25
0.50 0.65 1.10 |
●
● ● ● |
●
● ● ● |