ASTM A182, ASME B16.5
Sch 40S
Raised face, smooth finish (125-250 RMS / 3.2-6.3 µm) Product code example:FFSW-304L-2-150-40S |
Tube, pipe, fittings and flanges
Raised face, smooth finish (125-250 RMS / 3.2-6.3 µm) Product code example:FFSW-304L-2-150-40S |
Pipe | Flange | Hub | Raised face | Drilling template | Weight | Stock standard | |||||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Nom. size | O.D.1 | D | J | c | P | b | h | m | g | No. of holes | l | k | kg/pce | ASTM 304L | ASTM 316L |
in. | mm | mm | mm | mm | mm | mm | mm | mm | mm | mm | mm | ||||
1/2 3/4 1 1 ¼ |
21.3
26.7 33.4 42.2 |
88.9
98.6 108.0 117.3 |
22.4
27.7 34.5 43.2 |
15.7
20.8 26.7 35.1 |
9.7
11.2 12.7 14.2 |
11.2
12.7 14.2 15.7 |
15.7
15.7 17.5 20.6 |
30.2
38.1 49.3 58.7 |
35.1
42.9 50.8 63.2 |
4
4 4 4 |
15.7
15.7 15.7 15.7 |
60.5
69.9 79.2 88.9 |
0.42
0.59 0.81 1.07 |
●
● ● ● |
●
● ● ● |
1 ½ 2 |
48.3
60.3 |
127.0
152.4 |
49.5
62.0 |
40.9
52.6 |
15.7
17.5 |
17.5
19.1 |
22.4
25.4 |
65.0
77.7 |
73.2
91.9 |
4
4 |
15.7
19.1 |
98.6
120.7 |
1.36
2.10 |
●
● |
●
● |
1 O.D. = Outside Diameter