Superheater tubes and reheater tubes

Superheater tubes and reheater tubes in a comprehensive range of stainless steels and nickel alloys covering outside diameters 12 to 260 mm (0.472 to 10.24 in.).
Sandvik superheater tube and reheater tube materials cover all types of fuel, such as coal, gas, oil, black liquor and biomass. The Sandvik program also includes composite tubes consisting of two different alloys fully bonded together.
Increased efficiency in coal-fired power boilers
Our new material Sanicro 25 is engineered for the next generation of coal-fired power boilers, contributing to significantly greater efficiency and sharply lower CO2 emissions. It is ideal for superheater and reheater tubes, allowing for material temperatures of up to 700ºC (1290ºF). Read more about Sanicro 25.
Applications
Below are the most typical applications for Sandvik superheater and reheater tubes. Contact us for advice on product selection or other technical support.
Sandvik grade | Typical applications |
---|---|
Sanicro 25 (UNS S31035) |
Superheater and reheater tubes in the next generation of coal-fired power boilers for material temperatures of up to 700ºC (1290ºF). |
Sanicro 31HT (UNS N08811/N08810) |
Superheater and reheater tubes in boilers with corrosive conditions. |
Sanicro 41 (UNS N08825) |
Superheater and reheater tubes in boilers with corrosive conditions. Sanicro 41 is generally more resistant to flue gases compared to Sanicro 31HT. |
Sanicro 28 (UNS 08028, EN 1.4563) |
Radiant syngas coolers in IGCC gasification. Superheater tubes in boilers with corrosive conditions. The high chromium content of Sanicro 28 contributes to high gas corrosion resistance. |
Sanicro 30 (UNS N08800) |
Radiant syngas coolers in IGCC gasification. |
Esshete 1250 (EN 1.4982) |
Superheater and reheater tubes in sub-critical and supercritical coal-fired, biomass and other boilers. Sandvik Esshete 1250 has higher creep strength than most other alloys. |
Sandvik 7RE10 (UNS S31008/S31009) |
Superheater tubes in boilers with corrosive conditions. |
Sandvik 3R69 BT** (EN 1.4910) |
Superheater and reheater tubes in sub-critical and supercritical coal-fired boilers. |
Sandvik 8R61 (EN 1.4918) |
Superheater and reheater tubes in sub-critical coal-fired boilers and other boilers. |
Sandvik 6LR62 (UNS S31600/S31609) |
Superheater and reheater tubes in sub-critical coal-fired boilers and other boilers. |
Sandvik 8R41 (EN 1.4961) |
Superheater and reheater tubes in sub-critical coal-fired boilers and other boilers. |
Sandvik 8R40 (UNS S34709, ASTM 347H) |
Superheater and reheater tubes in sub-critical coal-fired, biomass and other boilers. Sandvik 8R40 can also be supplied in a fine-grain version. |
Sandvik 6R44 (UNS S34709, ASTM 347H) |
Superheater and reheater tubes in sub-critical coal-fired, biomass and other boilers. |
Sandvik 6R35 (UNS S32109, ASTM 321H) |
Superheater and reheater tubes in sub-critical coal-fired boilers and other boilers. |
Sandvik 5R10 (UNS S30409, ASTM 304H) |
Superheater and reheater tubes in sub-critical coal-fired boilers and other boilers. |
*Esshete 1250 is a trademark owned by Corus
Materials
Superheater and reheater tube materials (other grades can be offered on request)
Sandvik grade | UNS | ASTM | EN steel no. | EN name |
---|---|---|---|---|
Sanicro 251) | S31035 | - | 1) | - |
Sanicro 31HT2) | N08811/N08810 | 800HT | 1.4959 | X8NiCrAlTi32-21 |
Sanicro 41 | N08825 | (Alloy 825)5) | 2.4858 | - |
Sanicro 283) | N08028 | (Alloy 28)5) | 1.4563 | X1NiCrMoCu31-27-4 |
Sanicro 30 | N08800 | (Alloy 800)5) | 1.4558 | X2NiCrAlTi32-20 |
Esshete 12504) | S21500 | - | 1.4982 | X10CrNiMoMnNbVB15-10-1 |
Sandvik 7RE10 | S31008/S31009 | 310S/310H | 1.4845 | - |
Sandvik 3R69 | S31651 | 316N | 1.4910 | X3CrNiMoBN17-13-3 |
Sandvik 8R61 | (S31600/S31609) | (316H) | 1.4918 | X6CrNiMo17-13-2 |
Sandvik 6LR62 | S31600/S31609 | 316H | 1.4401 | X5CrNiMo17-12-2 215S51 |
Sandvik 8R41 | - | - | 1.4961 | X6CrNiTiB18-10 |
Sandvik 8R40 | S34709 | 347H | 1.4550/1.4912 | X7CrNiNb18-10 |
Sandvik 6R44 | S34709 | 347H | 1.4550/1.4912 | X7CrNiNb18-10 |
Sandvik 6R35 | S32100/S32109 | 321/321H | 1.4541/1.4940 | X7CrNiTi18-10 |
Sandvik 5R10 | S30400/S30409 | 304/304H | 1.4948 | X6CrNi18-10 |
1) Approved by VD TÜV 555
2) Approved by VD TÜV 434
3) Approved by VD TÜV 483
4) Approved by VD TÜV 520. Esshete 1250 is a trademark owned by Corus
5) Common name
Country | Standard | Specification |
---|---|---|
American | ASME SA213 ASTM A213 |
Seamless ferritic and austenitic alloy steel boiler, superheater and heat exchanger tubes. |
British | BS3059 BS3605 |
Steel boiler and superheater tubes. Seamless and welded austenitic stainless steel pipes and tubes for pressure purposes. |
European | EN 10216-5 | Seamless steel tubes for pressure purposes. |
French | NFS 49-214 | Steel tubes and seamless austenitic steel tubes for use at high temperatures. |
German | DIN 17459 AD Merkblatt W2 |
High temperature seamless circular stainless steel tubes. Materials for pressure vessels – austenitic steels. |
Japanese | JIS G3463 | Stainless steel boiler and heat exchanger tubes. |
Russian | TU 14-3-460-75E TU 14-3-796-79 |
Steam boiler tubes and pipe-lines of high or subcritical steam parameter equipment. |
Sizes and tolerances
Sandvik superheater and reheater tubes can be delivered in sizes and lengths according to below.
Outside diameter (OD)
12 to 260 mm (0.472 to 10.24 in.)
Wall thickness (WT)
2-20 mm (0.0787-0.787 in.)
Tolerances
Tolerances according to specification or according to agreement. Standard tolerances are:
Hot finished | OD +/- 1% | WT +/-12.5% |
Cold finished | OD +/-0.75% | WT +/-10% |
Lengths
Sandvik superheater and reheater tubes can be delivered in lengths up to 16 meters.