Sandvik’s welding consumables business has been acquired by ESAB from February 1, 2018. Over the coming months ESAB will be integrating the Sandvik portfolio, to provide a smooth transition for customers. During the integration period, the full line of Sandvik welding products will continue to be accessible on this website, or via the ESAB website.

ESAB Website

Please note that the Werkstoff Nr. corresponds to the base material of the same grade.

SandvikAWS* A5.4ISO 3581W.Nr.*Webshop
19.9.LR 308L-17 19 9 L R 1.4316
19.9.LB-15 308L-15 19 9 L B 1.4316
19.9.LR-16 308/308L-16 19 9 L R 1.4316
19.9.R-16 308/308H-16 19 9 R 1.4316
19.9.LR Cryo 308L-16 19 9 L R 1.4316
19.9.NbR 347-17 19 9 Nb R 1.4551
19.9.NbR-16 347-16 19 9 Nb R -
19.12.3.LB-15 316L-15 19 12 3 L B 1.4430
19.12.3.LR 316L-17 19 12 3 L R 1.4430 Buy product
19.12.3.LR-16 316/316L-16 19 12 3 L R 1.4430
19.12.3.LR Cryo 316L-16 19 12 3 L R 1.4430
22.12.HTR - - .
23.12.2.LR 309LMo-17 23 12 2 L R 1.4459
23.12.2.LR-16 309LMo-16 23 12 2 L -
24.13.R 309/309H-16 23 12 R -
24.13.LR 309L-17 23 12 L R 1.4332
24.13.LR-16 309/309L-16 23 12 L R -
29.9.R 312-16 29 9 R 1.4337
22.9.3.LR 2209-17 22 9 3 N L R 1.4462 Buy product
22.9.3.LB 2209-15 22 9 3 N L B 1.4462
25.10.4.LR 2594-16 25 9 4 N L R (1.4410) Buy product
25.10.4.LB 2594-15 25 9 4 N L B -
25.22.2.LMnB "310LMo-15"* 25 22 2 N L B (1.4466)
20.25.5.LCuR 385-16 20 25 5 Cu N L R (1.4519)
27.31.4.LCuR (383-16)* 27 31 4 Cu L R (1.4563)