Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 2XC24 is a martensitic stainless chromium steel.

Standards

  • ASTM: 410
  • UNS: S4100
  • EN Number: 1.4006
  • W.Nr.: 1.4006
  • SS: 2302
  • AFNOR: Z13C13
  • BS: 410S21

Certificates

Status according to EN 10 204 3.1

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.