Titanium tubing

Titanium tubing tubing suitable for environments and applications where the properties of stainless steels are not sufficient.
Haluatko lisätietoja?
Typical applications include tubing for the aerospace industry and heat-exchangers.
Sandvik titanium tubing is available in size range outside diameter 9.53–38.1 mm (3/8–1½ in.) with wall thicknesses from 0.7 to 5 mm (0.0275 to 0.1968 in.). The titanium tubes tubes are delivered in straight lengths or as U-bent tubes.
Grades and standards
Sandvik grade | UNS | ASTM/ASME | W.Nr. | AFNOR |
---|---|---|---|---|
Ti Grade 1 (CP Ti) | R50250 | Grade 1 | W.Nr. 3.7025 | T-35 |
Ti Grade 2 (CP Ti) | R50400 | Grade 2 | W.Nr. 3.7035 | T-40 |
Ti Grade 3 (CP Ti) | R50550 | Grade 3 | W.Nr. 3.7055 | T-50 |
Ti Grade 7 | R52400 | Grade 7 | W.Nr. 3.7235 | - |
Ti Grade 9 | R56320 | Grade 9 | W.Nr. 3.7195 | T-A3V2.5 |
Ti Grade 11 | R52250 | Grade 11 | W.Nr. 3.7225 | - |
Ti Grade 12 | R53400 | Grade 12 | W.Nr. 3.7105 | - |
Ti Grade 16 | R52402 | Grade 16 | - | - |
Ti Grade 17 | R52252 | Grade 17 | - | - |
Ti Grade 26 | R52404 | Grade 26 | - | - |
Ti Grade 28 | R52254 | Grade 28 | - | - |
Sandvik grade | Description |
---|---|
Ti Grade 1 (CP Ti) | Relatively low-strength and high-ductility pure titanium (Cp). |
Ti Grade 2 (CP Ti) | Medium-strength pure titanium (Cp). |
Ti Grade 3 (CP Ti) | High strength pure titanium (Cp). |
Ti Grade 7 | Medium-strength Pd-alloyed titanium for enhanced corrosion properties. |
Ti Grade 9 | High-strength titanium alloyed with 3% Al and 2.5% V. |
Ti Grade 11 | Low-strength titanium plus 0.12-0.25% Pd for enhanced corrosion properties. |
Ti Grade 12 | High-strength titanium alloy plus 0.3% Mo and 0.8% Ni for enhanced corrosion properties. |
Ti Grade 16 | Medium-strength titanium plus 0.04-0.08% Pd for enhanced corrosion properties. |
Ti Grade 17 | Low-strength titanium plus 0.04-0.08% Pd for enhanced corrosion properties. |
Ti Grade 26 | Medium-strength titanium plus 0.08-0.14% Ru for enhanced corrosion properties. |
Ti Grade 28 | High-strength titanium alloy plus 3% Al, 2.5% V and 0.08%-0.14% Ru for enhanced corrosion properties. |
Type of product | Grade(s) | Technical requirements* according to |
---|---|---|
Titanium tubes and pipes | Ti and Ti alloy grades 1, 2, 3, 7, 9, 11, 12, 16, 17, 26 and 28 | ASTM B337, ASTM B338, ASME SB338 NACE MRO 175-94 VdTÜV 230/2 Dimensional tolerances acc. to DIN 17861 D3/T3 or closer |
*Other requirements on request
Mechanical properties
Sandvik grade | UNS | Proof strength Rp0.2 MPa min | Tensile strength Rm MPa min | Elongation A % min |
---|---|---|---|---|
Cp Ti Grade 1 | R50250 | 138-310 | 240 | 24 |
Cp Ti Grade 2 | R50400 | 275-450 | 345 | 20 |
Cp Ti Grade 3 | R50550 | 380-550 | 450 | 18 |
Ti Grade 7 | R52400 | 275-450 | 345 | 20 |
Ti Grade 9 | R56320 | 483 | 620 | 15 |
Ti Grade 11 | R52250 | 138-310 | 240 | 24 |
Ti Grade 12 | R53400 | 345 | 483 | 18 |
Ti Grade 16 | R52402 | 275-450 | 345 | 20 |
Ti Grade 17 | R52252 | 138-310 | 240 | 24 |
Ti Grade 26 | R52404 | 275-450 | 345 | 20 |
Ti Grade 28 | R52254 | 483 | 620 | 15 |
Sizes and tolerances
Sizes and tolerances for titanium tubes
Sandvik titanium tubes are available in size range outside diameter 9.53-38.1 mm (3/8 - 1 1/2 in.) with wall thicknesses from 0.7 to 5 mm (0.0275 to 0.1968 in.)*.
OD = outside diameter
WT = wall thickness
Size OD, mm (in.) | Tolerances OD, mm (in.) | WT min wall % |
---|---|---|
< 25.4 (< 3/8) | ±0.102 (0.004) | +20/-0 |
25.4-38.1 (1-1 1/2) | ±0.127 (0.005) | +20/-0 |
Tolerances for OD < 15.9 or > 38.1 - or closer tolerances - after special agreement.
*Limitations for some ratios of OD/WT exist
Type of product | Grade(s) | Technical requirements |
---|---|---|
Titanium tubes and pipes | Ti and Ti alloy grades: 1, 2, 3, 7, 9, 11, 12, 16, 17, 26, 28 and 29 | ASTM B337, ASTM B338, ASME SB338 NACE MRO 175-94 VdTÜV 230/2 Dimensional tolerances acc. to DIN 17861 D3/T3 or closer |
Lengths
Titanium tubes are delivered in straight lengths up to 16.5 meters (54 ft). U-bent tubes are available on request.