Sanmac 304/304L

BarDatasheet

Datasheet updated 2020-12-10 06:47 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

General description

Sanmac 304/304L is an austenitic chromium-nickel steel with improved machinability.

Standards

  • ASTM: 304, 304L
  • UNS: S30400, S30403
  • EN Number: 1.4301, 1.4307
  • EN Name: X 5 CrNi 18-10, X 2 CrNi 18-9
  • W.Nr.: 1.4301
  • JIS: SUS304

Standards

Product standards

  • EN 10088-3, EN 10088-5 (dimensions up to 250 mm)
  • EN 10272, EN 10222-5, (dimensions ≥ 180 mm), AD-2000-W2
  • ASTM A479, A276
  • Chemical composition and mech. properties acc. ASTM A182

Approvals

  • TÜV AD-Merkblatt W0/TRD 100
  • Pressure Equipment Directive (2014/68/EU)
  • Ü-Zeichen
  • JIS Approval for Stainless Steel Bars

Certificate

  • Status according to EN 10 204/3.1

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.