Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sanmac 4435 is a molybdenum-alloyed (min. 2.5%) austenitic chromium-nickel steel with improved machinability.

Standards

  • ASTM: 316L, 316
  • UNS: S31603, S31600
  • EN Number: 1.4435, 1.4436
  • EN Name: X 2 CrNiMo 18-14-3, X 3 CrNiMo 17-13-3
  • W.Nr.: 1.4435, 1.4436
  • JIS: SUS316, SUS316L

Standards

Product standards

  • EN 10088-3, EN 10088-5 (dimensions up to 250 mm)
  • EN 10272, EN 10222-5, AD-2000-W2
  • ASTM A479, ASTM A276
  • Chemical composition and mech.properties acc ASTM A182
  • Basler Norm 2-1997

Approval

  • TÜV AD-Merkblatt W0/TRD 100
  • Pressure Equipment Directive (2014/68/EU)
  • JIS Approval for Stainless Steel Bars
  • Ü-Zeichen

Certificate

  • Status according to EN 10 204/3.1

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.