Sandvik 430 is a ferritic stainless steel with minimum 16% chromium that has lower tensile strength, elongation and impact resistance than austenitic stainless steels. The proof strength is somewhat higher.
Standards
-
ASTM: 430 -
UNS: S43000 -
EN Number: 1.4016
Certificates
Status according to EN 10 204 3.1
Chemical composition (nominal)
C | Si | Mn | P | S | Cr |
---|---|---|---|---|---|
≤0.035 | 0.3 | 0.3 | ≤0.025 | ≤0.025 | 17 |
Forms of supply
Sizes and tolerances
Round-cornered square, as well as round billets, are produced in a wide range of sizes according to the following tables. Larger sizes offered on request.
Surface conditions
Square billets
Unground, spot ground or fully ground condition.
Round billets
Peel turned or black condition.
Size | Tolerance | Length |
---|---|---|
mm | mm | m |
80 | +/-2 | 4 - 6.3 |
100, 114, 126, 140, 150 | +/-3 | 4 - 6.3 |
160, 180, 195, 200 | +/-4 | 4 - 6.3 |
>200 - 350 | +/-5 | 3 - 5.3 |
Sizes and tolerances apply to the rolled/forged condition.
Size | Tolerance | Length |
---|---|---|
mm | mm | m |
75 - 200 (5 mm interval) | +/-1 | max 10 |
>200 - 450 | +/-3 | 3 - 8 |
Size | Tolerance | Length |
---|---|---|
mm | mm | m |
77 - 112 (5 mm interval) | +/-2 | max 10 |
124, 134 | +/-2 | max 10 |
127, 147, 157 | +/-2 | max 10 |
142, 152, 163 | +/-2 | max 10 |
168, 178, 188 | +/-2 | max 10 |
183, 193 | +/-2 | max 10 |
Other products
- Hollow bar