Sanicro® 28

BilletsDatasheet

Datasheet updated 2020-12-10 06:47 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sanicro® 28 is a multi-purpose austenitic stainless ELC alloy for service in highly corrosive conditions. It is characterized by:

  • Very high corrosion resistance in strong acids
  • Very good resistance to stress and intergranular corrosion in various environments
  • Very high resistance to pitting and crevice corrosion
  • Good weldability

Standards

  • UNS: N08028
  • EN Number: 1.4563
  • EN Name: X 1 NiCrMoCu 31-27-4
  • W.Nr.: 1.4563
  • SS: 2584

Product standards

EN 10088-3

Certificates

Status according to EN 10 204 3.1

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.