Sanmac® 4435

BilletsDatasheet

Datasheet updated 2020-12-10 07:47 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sanmac® 4435 is a molybdenum-alloyed (min. 2.5%) austenitic chromium-nickel steel with improved machinability.

Standards

  • ASTM: 316L, 316
  • UNS: S31603, S31600
  • EN Number: 1.4435, 1.4436
  • EN Name: X 2 CrNiMo 18-14-3, X 3 CrNiMo 17-13-3
  • W.Nr.: 1.4435, 1.4436
  • DIN: X 2 CrNiMo 18 14 3

Product standards

  • EN 10088-3
  • ASTM A-314

Suitable for the production of flanges etc. according to ASTM A-182 Grade F316/316L.

Certificates

Status according to EN 10 204/3.1

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.