Sanicro® 28

Tube and pipe, seamlessDatasheet

Datasheet updated 2020-12-10 06:47 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sanicro® 28 is a high-alloy multi-purpose austenitic stainless steel for service in highly corrosive conditions. The grade is characterized by:

  • Very high corrosion resistance in strong acids
  • Very good resistance to stress corrosion cracking (SCC) and intergranular corrosion in various environments
  • High resistance to pitting and crevice corrosion
  • Good weldability

Standards

  • UNS: N08028
  • ISO: 4563-080-28-I
  • EN Number: 1.4563
  • EN Name: X 1 NiCrMoCu 31-27-4
  • W.Nr.: 1.4563
  • DIN: X 1 NiCrMoCuN 31 27 4
  • SS: 2584
  • AFNOR: Z1NCDU31-27-03

Product standards

Seamless tube and pipe: ASTM B 668, EN 10216-5, SEW 400 (Feb 1991), SS 14 25 84,
NFA 49-217
Plate, sheet and strip: ASTM B 709, EN 10088-2, SS 14 25 84
Bar steel: EN 10088-3, EN 10272, SS 14 25 84
Fittings: ASTM A 403 (chemical composition and mechanical properties according to ASTM B668)

Approvals

  • Approved by the American Society of Mechanical Engineers (ASME) for use in accordance with ASME Boiler and Pressure Vessel Code, section III, section I (Code Case 1325-18) and section VIII, division 1.
  • VdTÜV-Werkstoffblatt 483 (Austenitischer Walz- und Schmiedestahl)
  • NACE MR 0103 (Materials Resistant to Sulfide Stress Cracking in Corrosive Petroleum Refining Environments)
  • NACE MR0175/ISO 15156 (sulfide stress cracking resistant material for oil field equipment)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Send PDF via email