Sandvik 27.7.5.L

Welding wire Folha de dados

Folha de dados atualizada 2018-09-05 15:23 (substitui todas as edições anteriores)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 27.7.5.L is a filler material of hyper-duplex (austenitic-ferritic) stainless steel that has been specially developed for welding of the hyper-duplex steel Sandvik SAF 2707HD.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.