More nitric acid with less risk

Whether you’re refurbishing an older nitric acid plant or fabricating the process equipment to be used in one, selecting the right stainless steel tubing can be critical. High-quality tube with low impurities and optimized corrosion resistance will not only reduce downtime and extend your plant lifetime, but will allow for better welding and bending during manufacturing. Explore our special range of high-performance tube for nitric acid plants – and put our materials knowledge to work!

Need to know more?

Call us Email us

Risk reducing tube for nitric acid services

Having supplied material for hundreds of urea and nitric acid plants over the past 60 years, we’ve learned a lot about optimizing cooler condensers and more.

Many producers tell us they want higher alloyed grades than traditional 304L to combat higher temperatures, corrosion or oxidation issues. At the same time, they don’t want to invest heavily in expensive reactive metals. And engineering companies need materials that allow for faster and easier fabrication. Regardless of your specific engineering needs, Sandvik superior quality and material knowledge will offer you a competitive advantage – find out how!

Overview Sandvik range for nitric acid service

Chemical composition (nominal), %

Grade Material type UNS C Si P S Cr Ni Other
Sandvik 3R12 ASTM 304L S30403 ≤0.030 0.5 ≤0.030 ≤0.015 18.5 10 Mn 1.5
Sandvik
2RE10
ASTM 310L S31002 ≤0.015 ≤0.15 ≤0.020 ≤0.005 24.5 20 Mo ≤0.10 1.8
Sandvik SAF
2304®
- S32304 ≤0.030 ≤1.0 ≤0.035 ≤0.015 22.5 4.5

Mn ≤2.0, Cu
0.3, Mo 0.3 N
0.1