Knife steel

Annealed or cold-rolled knife steel in a wide range of stainless chromium steels delivered in coils or as straightened lengths belonging to the Sandvik SanEdge® portfolio. Sandvik's knife steel is used for the production of, for example:

Need to know more?

Call us Email us

  • Knives
  • Cutting parts for electric shavers
  • Pruning tools
  • Scissors
  • Skating blades

The Sandvik SanEdge® program of knife steel covers most requirements on material properties, which means that the most suitable knife steel for each application can be delivered. View mechanical properties for Sandvik's knife steels

Excellent blanking and hardening properties

Sandvik knife steels are characterized by fine microstructure and chemical composition within close tolerances. This results in excellent blanking and hardening properties, which facilitates trouble-free blade production and a high-quality end product.
Read more about important knife steel factors

Wide range of knife steel grades

The table shows Sandvik's wide range of knife steels including nominal chemical composition. View the material selection table below to find the best grade for each type of knife edge tool.

Sandvik grade C Cr Other Description
Sandvik
6C27
0.32
13.7
- A common knife steel grade with good corrosion resistance and low hardness, mainly used in applications where the need for wear resistance is low.
Sandvik
7C27Mo2
0.38
13.5
Mo 1.0
Generally the same properties as Sandvik 6C27, but with improved corrosion resistance.
Sandvik
12C27
0.60
13.5
- A knife steel with high hardness and good wear resistance.
Sandvik
12C27M
0.52
14.5
- A knife steel grade with good wear resistance and good corrosion resistance, well suited for the manufacture of kitchen tools.
Sandvik
13C26
0.68
13.0
- Generally the same properties as Sandvik 12C27, but with slightly higher hardness but less corrosion resistance.
Sandvik
14C28N
0.62
14.0
N 0.11 
Generally the same properties as Sandvik 12C27, but with higher hardness and slightly better corrosion resistance.
Sandvik
19C27
0.95
13.5
- A knife steel grade with very high hardness and wear resistance.
Sandvik 10C16Mo3V1
0.5
8.0
Mo 1.4 & V 0.3 The grade is suitable for tools and knifes in challenging applications such as garden tools and harvest knifes.
Sandvik 10C28Mo2
0.53
14
Mo 1.4 & N0.08 Suitable for kitchen knives and other tools where a dishwasher-safe material is required, professional butcher knives that need to be easily re-sharpened, outdoor knives, medical blades and razor blades, with high requirements on corrosion resistance and toughness.

Material selection table

Sandvik's wide range of knife steel makes it possible to select the most suitable knife steel for each application below.
Read more about choosing the right knife steel

Type of knife /application Sandvik
6C27
Sandvik
7C27Mo2
Sandvik
12C27
Sandvik
12C27M
Sandvik
13C26
Sandvik
14C28N
Sandvik
19C27

Sandvik 10C16Mo3V1 Sandvik 10C28Mo2
Bread knives - -
- - - - - -
Butcher's knives - -
- - - - -
Carpet knives - - - - -
-
Carving knives - -
- - - - - -
Chef's knives - -
- - - -
Circular knives
- - - -
Cutting heads* - - -
- - - -
Fishermen's knives -
- - - -
Folding knives - -
- -
- -
Frying slicers (spatulas) - - - - - - - -
Hunting knives - -
- - - - -
Ice drills - -
- - - - - -
Industrial knives -
- -
-
-
Kitchen knives - -
- - - -
Paper knives - - - -
- - -
Plastic film knives - - - - - - -
Pocket knives - -
- - - -
Pruning shears - -
- - - - -
Shaver knives* -
- - - - - - -
Skate blades - -
- - - - - -
Surgical knives - - - - - - - -
Synthetic fibre knives - - - -
-
-
-
Trimmers* - - -
- - - -

* For electric shavers

Hardening guide

Get expert advice on hardening of knife steel in Sandvik's hardening guide

Technical glossary

Our technical glossary explains the most important concepts.
Go to technical glossary